The 1700 and 1900 labels refer to MoSi2 element grades. For furnace selection, check the maximum element temperature separately from the furnace operating temperature. Confirm the limit for your furnace atmosphere and surface load. Ask for the test conditions before using the current and service-life figures below. See the 1900-grade MoSi2 product page for element shapes and sizes.
1700 and 1900 grade MoSi2 heating elements
- (1) The welding joint of 1900 Grade is full, protruding, bulging, and there is no crack in the welding place, which is very different from 1700 Grade.
- (2) The surface of 1900 Grade mosi2 heating element is smoother and has metallic luster.
- (3) Higher density, compared with 1700 Grade, the same specification of 1900 Grade mosi2 heating element will be heavier.
- (4) The operating current and voltage of 1900 Grade mosi2 heating element are smaller than those of 1700 Grade, for the same element with hot end of Diameter 9mm, the operating current of 1900 degree is 220A, while that of 1700 degree is about 270A.
- (5) Confirm the maximum element temperature for each grade under the same furnace conditions.
- (6) More shapes can be made according to customer requirements.
- (7) 1900 Grade mosi2 heating element is more solid, and generally will not break during transportation and installation.
- (8) Longer service life of 1900 Grade mosi2 heating element, generally more than 18 months

1700 and 1900 grade comparison
| السمة | 1900 Grade MOSI2 Heating Element | 1700 Grade MOSI2 Heating Element |
|---|---|---|
| Welding Joint | Full, protruding, bulging, no cracks | Different from 1900 Grade |
| Surface Appearance | Smoother, metallic luster | Different from 1900 Grade |
| الكثافة | Higher | Lower |
| الوزن | Heavier for the same specification | Lighter for the same specification |
| Operating Current and Voltage | Smaller | Larger |
| Current example (9 mm hot-end diameter) | 220A | ~270A |
| Maximum element temperature | Check the grade limit for the furnace atmosphere and surface load. | Check the grade limit under the same conditions. |
| Shapes Available | More shapes possible based on customer needs | Limited shapes |
| Durability | More solid, less prone to breakage | Potentially prone to breakage during transport |
| Reported service life | Generally exceeds 18 months | Varies, potentially shorter |